热水器加热管载荷下腐蚀研究

时间:2017-11-16 8:59:21  |  来源:深圳鑫盛发电热科技有限公司  |  作者: admin | 浏览:

关键词: 
加热管310S载荷态极化电阻Heating Tube 310S; Loading State; Polarization Resistance

摘要: 

用电化学线性极化电阻法研究了在载荷工况下,不同电力密度、氯离子浓度、碳酸氢根浓度、电导率对加热管310S不锈钢的腐蚀性能影响。从实验结果来看,水质对腐蚀的影响主要体现在加热和保温阶段。研究结果表明影响加热管使用寿命的环境影响因子由强到弱的排序为Cl > HCO3(结垢因子) > 电力密度,电导率对加热管腐蚀影响轻微。

The electrochemical linear polarization resistance method was used to study the effects of different power density, chloride ion concentration, bicarbonate concentration and conductivity on the corrosion performance of heating tube 310S stainless steel under loading state. From the experimental results, the impact of water quality on corrosion is mainly reflected in the heating and insulation stage. The results show that the order of environmental impact factors affecting the service life of heating tube is as follows: Cl > HCO3(scale factor) > power density (strong to weak), Conductivity has a slight effect on corrosion of the heating tube.
收藏  |  复制  |  顶一下(0)  |  踩一下(0)  |  更多:行业新闻    
电热产品 | 车间与设备 | 知名客户 | 常见问题 | 新闻资讯 | 关于我们 | 联系我们 | 网站地图 | 返回顶部
深圳市鑫盛发电热科技有限公司 版权所有 粤ICP备15095323号-1
地址:深圳市石岩镇园岭志泫翰工业园K栋2楼
联系电话:0755-29835076 传真:0755-29041770 E-mail:szxsf@szxsf.com
电热管,电加热管,3D曲面玻璃热弯机发热管,3D热弯机发热管,不锈钢电热管,单头电热管,发热架,电热膜 技术支持:中坚站